I've been using Briwax for some of our old furniture but am currently rather displeased to say the least.
Having used tins of various hues I found that the next time I opened the tin it had dried out. Later I got a clear one, used it, then replaced the lid
firmly like I've always done then waited a mo.' Yes, the lid slowly raised up on one side. Hmmm. Did this several times and virtually stamped on the blasted thing and after 10 minutes all was well. A few months later I came to use it and guess what. It had all dried out! I know it's the volatile solvents escaping but why don't they supply those metal clips you put on the side of the tin and lid to stop it doing this? Anyone know of a better product that does the biz?